Acid Ditch Repair Project
|
Highlights
When: September 2004 Ambient
environment: Chemicals used in processing kaolin including
acids and bleaches Original completion
date: circa 1985 Contractor: Topcor (Augusta,
GA) Concrete supplier: All-Star Concrete Top
coat: Ceilcote (Atlanta, GA)
Before Repair
Concrete in an aggressive environment can
weaken and fail quicker than expected. This
structure is in an environment with acids
and bleaches, and was in need of repair.
|
 |
Cement:
KAOROCK™:
Fine aggregate:
Coarse aggregate:
Total water (incl. absorbed):
Air entraining agent:
ADVA HRWRA:
|
667 #/cy
55 #/cy
1,046 #/cy
1,917 #/cy
325 #/cy
1.00 cf
added for 4” slump
|
Water/cementitious
materials ratio = 0.45
Aggregate as % of total volume = 67%
|
While
repairing the ditch, the concrete
mix was very easy to handle and it finished
great. Along with added strength and
durability, KAOROCK assists the contractor
in finishing the job.
|

During the repair |

After the repair |
|
® Thiele
Kaolin Company 2005 P. O. Box 1056, 520 Kaolin
Road, Sandersville, GA 31082 USA
|
|
Phone:
(478) 552-3951 Fax: (478) 552-4131
|
|
|